| NAME:Wenqing   QU    GENDER:Male DATE of BIRTH:Feb.   1, 1972 TITLE:Associate Professor, Beijing University   of Aeronautics & Astronautics(Beihang University) ADDRESS:No. 37 Xueyuan Road, Haidian District, Beijing City, China WORK PHONE: 86-10-82317702 MOBILE PHONE:13701172912 EMAIL:quwenqing@buaa.edu.cn EDUCATION   Sep. 1997 — Dec. 2000   Beihang    University,   Ph.D, Mechanical   Engineering & Automation   Sep. 1994 — July 1997      Beihang    University,   Master, Welding      Sep. 1990 — July 1994   Beihang    University,   Bachelor, Welding   Process & Equipment                   WORK EXPERIENCE   Dec. 2014-Dec.2015      Visiting Scholar, University of Western   Antario, Canada Since Sep. 2003        Associate   Professor, School of Mechanical Engineering & Automation(SMEA),Beihang    University Since Jan. 2003       Staff   (Deputy Dean for Graduate Studies), SMEA, Beihang  University Jan. 2001-Dec. 2002    Post-Doctor Researcher, SMEA, Beihang    University   RESEARCH INTERESTS   1、Brazing      Vacuum Brazing of non-metal with metal The vacuum brazing   process of Carbon fiber composites jet tube and niobium alloy using   copper-free silver base filler metal was developed, and the laminate injector   of stainless steel(or Titanium alloy) was also vacuum brazed, and the heat   run had been passed in shanghai in 2009, shown as Fig.1.   
     High Frequency Induction Brazing of   dissimilar metals The brazing processes   of dissimilar metals tube such as Aluminum alloy with stainless steel,   Aluminium alloy with Titanium alloy, Titanium alloy with stainless steel were   developed, and three patents for invention were authorized, shown as Fig.2. These   technologies were used in the validation structure of the tube structures in a   certain satellite propulsion subsystem. The brazed tube structures of   Titanium alloy with stainless steel were used in the heat exchanger liguate   tube of a certain launch vehicle, shown as Fig.3.     Other Brazing Processes of Special   structures The High frequency   induction brazing processes of Aluminum alloy square tube with stainless   steel tube was developed. After 24 hours marinating in liquid nitrogen, the leak rate of brazed   joint is lower than 1×10-10Pa.m3/s, shown as Fig.4. The locule   leak detection assembly is the key equipment which detecting whether the rendezvous   and docking is successfully or not in the first mission of manned space   flight project. We completed the optimization of structure design, and   developed the brazing technology of the locule leak detection assembly. This   technology has been used in the mission of rendezvous and docking of No. 8,   No. 9, and No. 10 of Shenzhou spaceship with No. 1 of Tiangong spacecraft,   shown as Fig.5. 
 2、Soldering     Large Area Soldering for Loop Heat Pipe vaporizer structures As the most important   component of LHP(Loop Heat Pipe), the evaporator consists of aluminum alloy saddle   seat and stainless steel heat collection pipe. Using the large area soldering   process, the aluminum alloy saddle seat and stainless steel heat collection   pipe was bonded together. The thermal property is higher nearly ten times   than that of the evaporator glued joint by the thermally conductive adhesive.   The relevant research results have been applied two patents of invention. Two   types of LHP vaporizer brazed structures has been used in the thermal control   subsystem of certain satellite and spacecraft. 
  Low temperature interface diffusion bonding   Process Supported by the superpower   and high density of heat flow interface heat transfer enhancement technology,   now a new low temperature interface diffusion bonding technology was   invented, it can be achieved that bonded at 80℃   but not remelted over 250℃. And the thermal   conduction of the interface bonded structure is over 10 times than that of glued   interface by the thermally conductive adhesive, shown as Fig.7. The relevant   research results have been applied two patents of invention.  Solder Sealing Process of inertial   instrument system The High frequency   induction soldering process and the equipment for the aluminum alloy inertial   controlling device were developed. The inertial controlling unit can be   solder sealed in tens seconds, the heating time is shorter than that using   iron, so good quality and productivity can be achieved, shown as Fig.8.  
   3、Special Active Welding   Process     The new DCSP-TIG welding process of   Aluminum alloy Well known, The   porosity is the worst problem of Aluminum alloy welding, and Aluminum alloy   can not be welded by DC straight polarity (DCSP) TIG welding process, because   the compact Al2O3 layer covers on the surface of   Aluminum alloy. A new DC straight polarity TIG welding process for Aluminum   alloy was developed to wipe away the welded porosity, and 7 patents of   invention had been applied. New brazing flux was used to remove Al2O3   and H2 pore in the welding process. No porosity appeared in the   welded seam, and the joint property and productive efficiency were elevated,   shown as Fig.9. 
     Active Friction Stir Welding(Soldering)   Process S line is the defect   difficult to avoid from FSW seam of Aluminum alloy, caused by Al2O3   layer. The new active FSW process was developed to avoid the appearance of S   line,shown   as Fig.10. And another active friction stir welding/Soldering process was   developed for Aluminum alloy wall panel to improve the fatigue property of   Aluminum alloy FSW joint. The relevant results have been applied two patents   of invention. 
     Low-Temperature Metal Bonding process Many problems exist   in the Thermally Conductive Adhesive and conductive adhesive, such as poor heat   and electric conduction, short time in service etc. A new metal bonding   process has been developed as the replacer of thermally conductive adhesive   and conductive adhesive, many metals such as Aluminum alloy, stainless steel,   Titanium alloy and copper can be bonded under the temperature of 100℃, with the advantage of excellent heat   and electric conduction, long time in service.     Active Soldering process The process for   directly bonding ceramic with metal in air was developed, one patents of   invention have been authorized.   4、Microstructures and Properties of bonded   joints     Microstructures and Properties of 2219   welded joints 2219 aluminum alloy   is the conduithead body metal of china new launch vehicle, its   microstructure, property and welding performance has the most important   effect on the safety of the welded conduithead. So the microstructures,   mechanical properties, and fracture properties of base metal and the welded   joints of two heat treatment state(T62, T87) 2219 Aluminum alloy were   studied, the welded joints include the variable polarity TIG (VP-TIG) welded   joint, variable polarity plasma arc (VPPA) welded joint, friction stir welded   (FSW) joint, and FSW/VPPA cross welded joint. The results have the important   significance to the welding and safe assessment of launch vehicle conduithead. 
     Microstructures and Properties of Aluminum   alloy FSW joints The microstructures and properties of FSW   joint of Aluminium alloy(such as 2024, 7050, 6082, Al-Li-S-4 alloy etc) were   studied, including tensile strength, impact toughness, fracture toughness, fatigue   property, shown as Fig.12 and13.   
  
 
     Microstructures and Properties of Brazed   joints in electron device The microstructures   and properties of brazed joints of vacuum electron device were studied.  Many materials combinations were used in   the vacuum electron device, such as oxygen-free copper, stainless steel,   iron, Monel, kovar alloy. They are all brazed together in the vacuum electron   device, so their microstructures and properties were obtained in order to   direct structural design and optimizing of process.      Complex Thermal-mechanical environmental   assessment of golden alloy soldered joint in aerospace control subsystem The microstructures   and properties of soldered joints of golden alloy in aerospace control   subsystem in complex thermal-mechanical environment were studied, including   room temperature tensile test, room temperature creep test, high temperature tensile test, high-low   temperature cyclic test, high temperature storage test. The soldered joints   include SnPb soldered joint, InPb soldered joint, and InPbAg soldered joint.  
   |